看起來你不是TradeKey.com的會員。 立即註冊,與全球超過7百萬的進口商和出口商建立聯繫。 立即加入 |
BOOK A CALL
Book Call On Your Favorite Time
Code
🗘

By Signing Up. I agree to TradeKey.com Terms of Use, Privacy Policy, IPR and receive emails related to our services

Contact Us
product
Prev
Cemented Carbide Welding Cutting Blade Tips
Next

Cemented Carbide Welding Cutting Blade Tips

离岸价格

获取最新报价

32 ~ 68 USD / Kilogram

|

20 Kilogram Minimum Order

国家:

China

型号:

-

离岸价格:

32 ~ 68 USD / Kilogram 获取最新报价

位置:

-

最小订单价格:

32 per Kilogram

最小订单:

20 Kilogram

包装细节:

as to buyer's requirements

交货时间:

5-25 days

供应能力:

50000 Kilogram per Month

付款方式:

-

现在联系

联系人 Melon

Chongqing, Chongqing

现在联系

产品规格

  • Brand Name: Henghui

详情

1. The welding cutting tool structure should have sufficient rigidity.

Sufficient rigidity based on the maximum allowed size and shape and higher strength steel and heat treatment.

 

2. Cemented carbide inserts should be fixed firmly.

Carbide welding inserts should be a sufficient degree of fixed firm, which is relied on slot and weldingquality to guarantee. Therefore, you should to select the  shape of the insert slot according to the bladeshape and tool geometry parameters.

 

3. Examine arbor carefully.

To carry out the necessary checks to blade and arbor before blades welded to the shank. 

First, you should check the blade bearing surface, make sure it can not be serious bending. 

Second, the carbide welding surface may not have serious carburized layer. 

Last, clear dirt carbide blade surface and arbor insert slot to ensure solid welding.

 

4. Select solder reasonably.

In order to ensure the weld strength, you should choose a suitable solder. In the welding process, you should ensure good wetting and flow, and the exclusion of air bubbles, make sure welding full contact with alloy welding face and no shortage of welding phenomenon.

 

5. Choose welding flux rightly.

It is better to use industrial borax and dehydrated in a drying oven before use, then crushed andsieved to remove mechanical debris and set aside.

 

6. Net form shim.

In order to decrease the welding stress in high titanium low cobalt fine particle alloy welding, and long and thin alloy blade welding, we suggest to using slice with thickness of 0.***0.5mm or Net form shim with bore diameter of ***3mm as compensate shim.

 

7. Right way of cutter sharpening.

Since carbide chip are of good brittleness, and are sensitive to crack formation, so it should be avoid overheating or quenching during the cutter sharpening. Meanwhile, to avoid flawing and shorten service life of the tools, it should choose abrasion wheel with suitable particle size and reasonable grinding technology.

 

8. Right way of tool installing.

Cutter bit extend length of knife rest should as short as possible, or it will result in tool shaking and thereby damaging the alloy slice.

 

9. Right way of regrinding, grinding tool.

When it reach normal blunt, tools should be regrinded. After regrinding, it is necessary to polishing cutting edge and fillet with abrasive store. It can increase service life and safe reliability.

国家: China
型号: -
离岸价格: 32 ~ 68 / Kilogram 获取最新报价
位置: -
最小订单价格: 32 per Kilogram
最小订单: 20 Kilogram
包装细节: as to buyer's requirements
交货时间: 5-25 days
供应能力: 50000 Kilogram per Month
付款方式: -
產品組 : tungsten carbide tool
Cemented Carbide Welding Cutting Blade Tips

Send a direct inquiry to this supplier

至:

Melon < Chongqing Henghui Precision Mold Co., Lt >

我想知道: