Application method:
Paper making:
1. When brighten in pulp, BA should be added before alum or
cationic auxiliary agent; Dosage: 0.***0.4% (of absolute dry
pulp).
2. In surface sizing, it can work with CMC, PVA, starch, or anionic
or weak cationic synthetic sizing agent.
3. In coating, it can be used at any stage of coating production in
the form of aqueous solution after dissolved.