看起來你不是TradeKey.com的會員。 立即註冊,與全球超過7百萬的進口商和出口商建立聯繫。 立即加入 |
BOOK A CALL
Book Call On Your Favorite Time
Code
🗘

By Signing Up. I agree to TradeKey.com Terms of Use, Privacy Policy, IPR and receive emails related to our services

Contact Us
Sell master alloy for goldsmith's, GYS34 Suit for 18K in yellow gold

Sell master alloy for goldsmith's, GYS34 Suit for 18K in yellow gold

离岸价格

获取最新报价

|

Minimum Order

位置:

China

最小订单价格:

-

最小订单:

1 Kilogram

包装细节:

Plastic bottle in carton

交货时间:

within 3 days

供应能力:

6000 Kilogram per Year

付款方式:

T/T, Western Union, Money Gram

现在联系
免费会员

联系人 Tony

No1. GuangXing Road, DaYan Industrial Park, HuangPu Town, Zhongshan, Guangdong

现在联系

详情

 
Application
Karat *8K Color 3N Yellow
Application C, C/S Special Low melt loss, Less porosity
Lower price
Composition *4%Ag    
 
Color
karat L * a *   b *
*8K 3N *8.*4 4.*8
   
Characteristics
  Density [g/cm^3] Hardness [HV]   Melting range [° C]
*8K *5.*8 **2 ******0
 
Castingtemperature: Suggesttemperature: *******0° C
F lasks temperature: Suggest temperature: ******0° C
Help-solvent: Suggest using borax as help-solvent, for casting by machine don’ t need it.
Set down casting temperatureaccording to the identity of product, lower flasks temperature for layer product; higher flasks temperature for lighter product.
Suggest advance-melting before casting, and make sure melting well-proportioned.
 
 
Water Cooling
Cooling in the air for ****0 minutes before water cooling, more cooling time in the air for the layer product.
 
Cleaning
Using high pressure water to cleaning the plaster, and than put the product into ***0% hydrofluoric acid in order to cleaning the residual plaster.
 