详情
The main ingredients:
TiO2 ≥*2
S ≤0.**5
P ≤0.*4
FeO ≤0.5
C ≤0.2
The faction in the material of welding :
Advantage:
easy to deoxidating ,contain about *0% Fe
electric arc is steady ,molten pool is tranquil
Add or improve the deposition efficiency
make the welding line more beautiful ,and good slag cover
disadvantage:
overcommit will be difficulty in producing the welding
electrodes
soldering block temperature will be high ,slag will be rare
The influence of the welding process performance:
Along with the FeO content is increasing in reduction ilmenite ,
the performance of welding process parameters will be affected.The
test results show that the coarse is slightly better than thin