Simple description of liquid silicone rubber
Hongye liquid silicon rubber is white or red flowing liquid with general hardness of 22-50A°after curing. Hongye mold making liquid silicon rubber is a kind elastic silicon rubber mold
which features with resistance to deformation, high-temperature, acid-alkali and
expansion as well as high reproduction times, good tensile strength, tear strength and elongation.
Application of liquid silicone rubber
A Decorative items: cornices, columns, ornaments, statues
B Figurines: toys, candles, giftware, soap, craft projects, sculpture
C Furnishing: casting of furniture and decoration
D Construction: prefabrication of decorative features, pavement, paving stone, urban furniture,concrete casting
liquid silicone rubber datasheet
Model |
Color |
Mixing ratio |
Pot life (mins) |
Demouled time (hrs) |
Hardness(A0) |
Tensile-strength ((kgf /cm2 ) |
Tear-strength KN/m) |
Viscosity (mPa.s) |
Elongation (%) |
Shrinkage rage (%) |
HY625 |
white |
100:3 |
30-50 |
5-6 |
20±2 |
≥30 |
≥22 |
≤18000 |
410 |
0.3 |
HY625 |
white |
100:3 |
30-50 |
5-6 |
25±2 |
≥32 |
≥25 |
≤20000 |
410 |
0.3 |
HY630 |
white |
100:3 |
30-50 |
5-6 |
30±2 |
≥28 |
≥28 |
30000~38000 |
410 |
0.3 |
HY635 |
white |
100:3 |
30-50 |
5-6 |
35±2 |
≥38
|
≥28 |
≤38000 |
410 |
0.3 |
Features
of liquid silicone
rubber
(1) Silicon rubber for mold making with SGS and ROSH approval
(2) Curing agent arrange together as free charged
(3) In liquid form and in various colors
(4) With an exceptional fluidity and good operability.
(5) Temperature and deformation resistance as well as low
shrinkage.
(6) High duplication times.
(7) Sample orders are available
(8) MOQ: 200KG
Why does the silicone mold get burnt out?
This consequence happens only because you have left out the important notes when using unsaturated
resin materials to produce your products. The unsaturated resin produces great heat when added the curing agent. So you must demould the product within 3 minutes to avoid this problem.
1. 5kg/drum, 20kg/drum, 25kg/drumor 200kg /drum.
2. It is a kind of non-dangerous goods, and it should be stored at a cool and dry place,
please keep it from sun and rain