Magnesium cement has low alkaline (PH **9). Large chloride content,
large modifier content, fast consolidation characteristics.
Magnesium cement needs foaming agent adaptive to low alkalinity,
chloride-resistant, not effected by modifier, as well as large
output. Magnesium Oxide foaming agent is developed to meet
magnesium cement characteristics.
Water Diluent: *0 times Output: 1L Magnesium Oxide foaming agent
generates *******0L foam. PH: **9 Density: 1.*5 Color: light
brownish liquid Packing: **0kg/barrel, ***0kg/barrel Storage: *2
months. Cool place, no direct sun Application: fireproof door, door
fill-in, light weight Magnesium Oxide wall board.