High speed steel roll ring contained W*6%, C2.4%, the tonnage achieved per slot compared with the high Ni-Cr chilled roll increases almost 5~7fold, it’s life time be equal to that of import goods, but the price is 1/**1/5 of the latter.
Main chemical composition:
C:2.0~2.4%,W:*2~*6%,Mo:2~3%,V:4~7%,Cr:2~4
Mechanical properties:
ak:5~*0J/cm2, σ b:**0~**0MPA, HRC:*0~*2.