联系人 Ms. Olivia
Han Kow north Road, Wuhan, Hubei
Construction technology progress of acrylic acid sports
court
1. Bottom glue: mix glue and water with proportion of 1:2, which
means that every *0kg glue mixed with *0kg water, then glue the
mixture on ground with roller.
2. Floating coat: the dosage of floating coat is about 0.4kg per square. One big barrel is often divided into three small barrel. And the proportion of floating coat and sand is 1:1, the weight of every small barrel is 0.**0.5kg, that means every one big barrel of floating coat is *5kg, which is divided into three small barrel with weight of 8.*3kg, then we add 8.*3kg sand into one small barrel and 0.5kg cement.
3. The second time to spray finishing paint: One barrel finishing paint is divided into two small barrer, and add about 1kg water into every one small barrer.
4. Finishing construction of all progress, after 7days for maintenance, then we can put it into use.